The chart below shows how different plating materials react to one another with regard to their galvanic potential.
													
																	Nickel plating aluminum galvanic corrosion. 
									
																	Typically we are plating small precision machined housings from 6061 t6 aluminum alloy. 
																	Galvanic corrosion is an electrochemical process in which one metal corrodes preferentially to another when both metals are in electrical contact in the presence of an electrolyte. 
																	Note that ni is more noble than low carbon steel essentially iron and. 
																	Electroless nickel plating en can be applied to a wide range of basis metals including steel copper brass and aluminum alloys. 
															
													
									
																	The plating is typically electroless nickel and then gold. 
																	I am having plating problems such as visible peeling and blistering and voiding in areas. 
																	First there must be two electrochemically dissimilar metals present. 
																	Porosity in base metal causing plating problems february 3 2017. 
															
													
									
																	Galvanic corrosion some times called dissimilar metal corrosion is the process by which the materials in contact with each other oxidizes or corrodes. 
																	Galvanic corrosion also called bimetallic corrosion or dissimilar metal corrosion is an electrochemical process in which one metal corrodes preferentially when it is in electrical contact with another in the presence of an electrolyte a similar galvanic reaction is exploited in primary cells to generate a useful electrical voltage to power portable devices. 
																	Iron group metals nickel cobalt iron nickel plating is among the most common electrodeposition processes and is used mostly as a part of a multilayered system designed to increase wear and corrosion resistance and also able to function as a diffusion barrier.